Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX9400W - Americas - (PPE+PA*) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX9400W - Americas:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl GTX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
NORYL GTX™ 9400W resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA) that exhibits high heat resistance, high flow, and added mold release. NORYL GTX9400W resin is injection moldable and an excellent candidate for automotive under-the-hood applications such as power distribution boxes, relay boxes, connectors, sensors, and fuse box covers.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 97 g/10min ASTM D 1238
Temperature 280 °C -
Load 5 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 69 MPa ISO 527
Strain at break 39 % ISO 527
Flexural modulus 2700 MPa ISO 178
Izod notched impact strength, +23°C, 4mm 21 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 1950 MPa ASTM D 638
Tensile Strength at Yield 64 MPa ASTM D 638
Tensile Strength at Break 62 MPa ASTM D 638
Elongation at Yield 11 % ASTM D 638
Elongation at Break 40 % ASTM D 638
Izod Impact notched, 1/8 in 256 J/m ASTM D 256
Izod Impact notched, Low-Temperature 112 J/m ASTM D 256
Temperature -30 °C -
Izod Impact unnotched, 1/8 in 849 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 78 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 187 °C ISO 75-1/-2
Vicat softening temperature, B 203 °C ISO 306
ASTM Data
DTUL @ 66 psi 190 °C ASTM D 648
DTUL @ 264 psi 83 °C ASTM D 648
Vicat Temperature 212 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 1100 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 95 - 105 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.07 % -
Melt temperature 270 - 295 °C -
Mold temperature 65 - 95 °C -
Zone 1 255 - 295 °C -
Zone 2 260 - 295 °C -
Zone 3 265 - 295 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 1.4 MPa -
Characteristics
Processing
Injection Molding
Applications
Automotive
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.